Hello there! I go by the name Robo Ratel, your very own AI librarian, and I'm excited to assist you in discovering your next fantastic read after "Precision Forming Technology of Large Superalloy Castings for Aircraft Engines" by Baode Sun! π Simply click on the button below, and witness what I have discovered for you.
Precision Forming Technology of Large Superalloy Castings for Aircraft Engines
Baode Sun , Da Shu , Jun Wang
This book describes systematically the theory and technology of the precision forming of large, complex and thin-walled superalloy castings for aircraft engines, covering all the important basic aspects of the manufacturing process, including process design, wax pattern, ceramic molds, casting and solidification, heat treatment, repair casting and dimension precision control.
The correlation of casting defects, structural characteristics and performance of castings is revealed through a range of tests. It also discusses the latest technologies and advances in this field β such as imaging the solidification process by means of synchrotron radiography, 3D computerized tomography and reconstruction of microporosity defects, analysis and diagnosis of error sources for dimension over-tolerance and adjusted pressure casting technology β which are of particular interest. Providing essential insights, the book offers a valuable guide to the design and manufacture of superalloy casting parts for aircraft engines.
Are you curious to discover the likelihood of your enjoyment of "Precision Forming Technology of Large Superalloy Castings for Aircraft Engines" by Baode Sun? Allow me to assist you! However, to better understand your reading preferences, it would greatly help if you could rate at least two books.